Header banner
Revain logoHome Page
πŸ’‘ 2oz flat jar of chip quik ra891 rosin solder flux (ra) - 50g logo

πŸ’‘ 2oz Flat Jar of Chip Quik RA891 Rosin Solder Flux (RA) - 50g Review

5

Β·

Average

Revainrating 3 out of 5Β Β 
RatingΒ 
3.0
πŸ”¨ Welding Tools, πŸ”§ Automotive Tools & Equipment

View on AmazonView on Π―M

Media

(2)
img 1 attached to πŸ’‘ 2oz Flat Jar of Chip Quik RA891 Rosin Solder Flux (RA) - 50g
img 2 attached to πŸ’‘ 2oz Flat Jar of Chip Quik RA891 Rosin Solder Flux (RA) - 50g

Description of πŸ’‘ 2oz Flat Jar of Chip Quik RA891 Rosin Solder Flux (RA) - 50g

Rosin Activated. ROM1. Solder Flux.

Reviews

Global ratings 5
  • 5
    2
  • 4
    0
  • 3
    1
  • 2
    0
  • 1
    2

Type of review

Revainrating 1 out of 5

Buy American: Welding and Soldering

There's good stuff here folks! A super high quality flux that has left my solders pristine. Support American companies!

Pros
  • Absolute Legend
Cons
  • Almost Everything Is OK

Revainrating 5 out of 5

Good product in the soldering flux category

Disappointed by several "fluxes" with rave reviews, I finally settled on this one. Good decision. The plastic container could not hold more product. My iron likes it. My boards love it. Even my old fashioned 63-37 eutectic solder likes it. By the way, do you know why eutectic solder is so much better than 60-40 or any lead-free solder? Because it has no plastic step when heated. It's either solid or liquid, nothing in between. With eutectic solder you get perfect, clean and shiny solder joints.

Pros
  • Sample for a year
Cons
  • I won't say anything

Revainrating 5 out of 5

Good product!: Soldering and soldering equipment

I am satisfied with the product and the seller too. I had an issue with the delivery man leaving me and an empty bag but I call customer service and they resend the item.

Pros
  • Soldering flux
Cons
  • Other Other

Revainrating 1 out of 5

Dry and hard soldering flux

It is dry and solid; cannot be traced back to noodles. Gave him a few days indoors, thinking the heating might help, but to no avail. Correct distribution at the soldering points is not possible. The date of manufacture on the case is September 2021, so it is not old stock, but a question of composition.

Pros
  • Welding and brazing
Cons
  • Other

Revainrating 3 out of 5

It works, but it's hard as a rock.

Can be an effective flux. But the only real use I've found for it is to impregnate the wicks to remove solder and for that I have to put my soldering iron in a container of flux to melt it first because at the same time it's so hard that You will need a screwdriver to scrape off some of the flux. This and yet, unlike most phlox, once it's been used on something it doesn't turn into a hard shell that can be easily chipped off, it remains almost the same very hard but slightly sticky consistency…

Pros
  • Solder and Flux
Cons
  • Fine