Header banner
Revain logoHome Page
Frank Dubey photo
1 Level
1331 Review
43 Karma

Review on JacksonLea 47326SP Buffing Compound Standard by Frank Dubey

Revainrating 1 out of 5

doesn't do what it's supposed to

The text says it cuts metals, including aluminium, quickly. It leaves a residue on annealed 6061 aluminum that can only be removed with a solvent such as naphtha. Because it covers the surface with this residue, the metal is protected from any further abrasive action of the rod. Tried with sisal and sewn wheel with same problem.

Pros
  • Steel Polishing Paste: Used with HY treated loose and sewn regular polishing pads
Cons
  • write later