I had vertical and horizontal welding for about 1 week. I made a custom grid for my uncle and when I boiled vertically the slag from the flux core built up on it and started to melt and destroyed the nozzle. Now half the nozzle is only a week away from welding. Not recommended, I wish they made it out of some kind of metal, I don't understand why they make it out of plastic when we are working at very high temperatures.